University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
9 results
Search Results
Item type:Publication, Evaluation of reactive induction sintering as a manufacturing route for blended elemental Ti-5Al-2.5Fe alloy2018, ElsevierThis work focuses on gaining a better understanding of the feasibility of using reactive induction sintering to obtain the alloy Ti-5Al-2.5Fe using Ti, Al and Fe powders (i.e. via a blended elemental approach). For this, powder compacts were induction sintered under various temperature/time combinations like 700–1250 °C and isothermal holding of 0–15 min. Compositional homogeneity, microstructure evolution and mechanical properties of the sintered Ti-5Al-2.5Fe alloy were investigated. It was found that by increasing the sintering temperature and isothermal holding time, sintered Ti-5Al-2.5Fe components with a homogeneous chemical composition and a Widmanstätten microstructure can be produced. The tensile strength increases with the sintering temperature/time reaching comparable values to the wrought alloy; however the residual porosity has a significant impact on the ductility of the alloy. This study demonstrates that reactive induction sintering is suitable to shorten the production route of blended elemental Ti alloys to be used in non-critical applications where ductility is not the main requirement.Item type:Publication, Low-Cost α+β PM Ti Alloys by Fe/Ni Addition to Pure Ti2016Ti and its alloys can deliver a very interesting combination of properties such as low density, high strength, corrosion resistance and biocompatibility and, therefore, are very flexible materials which can be adapted to various applications. Nonetheless, Ti and Ti alloys are only employed in critical applications (i.e. aeronautical and aerospace, nautical, medical, etc.) or in products for leisure. In both of these cases the higher fabrication costs of Ti in comparison to its competitors (i.e. steel and aluminium) is not the limiting factor as it is for many structural applications, especially for mass production (i.e. automotive sector). The use of creative techniques and the decrement of the starting price of Ti have been identified as the two main routes to follow to decrease the fabrication costs. In this study, the production of low-cost α+β Ti alloys has been assessed by combining the addition of cheap alloying elements (in particular a Fe/Ni powder) with the classical powder metallurgy route (pressing and sintering). Physical and mechanical properties as well as microstructural analysis of these low-cost alloys were measured and correlated to the processing parameters used to sinter them. It is found that the low-cost Ti alloys show similar behaviour to conventional α+β Ti alloys and, thus, have the potential to be used for non-critical applications.Item type:Publication, Quantifying the properties of low-cost powder metallurgy titanium alloys2017-02The extensive industrial employment of titanium is hindered by its high production costs where reduction of these costs can be achieved using cheap alloying elements and appropriate alternative processing techniques. In this work the feasibility of the production of low-cost titanium alloys is addressed by adding steel to pure titanium and processing the alloys by powder metallurgy. In particular, a spherical 4140 LCH steel powder commonly used in metal injection moulding is blended with irregular hydride-dehydride Ti. The new low-cost alloys are cold uniaxially pressed and sintered under high vacuum and show comparable properties to other wrought-equivalent and powder metallurgy titanium alloys. Differential thermal analysis and X-ray diffraction analyses confirm that Ti can tolerate the employment of iron as primary alloying element without forming detrimental TiFe-based intermetallic phases. Thus, the newly designed α+β alloys could be used for cheaper non-critical components.Item type:Publication, Evaluation of the mechanical properties of powder metallurgy Ti-6Al-7Nb alloy2017-03Titanium and its alloys are common biomedical materials owing to their combination of mechanical properties, corrosion resistance and biocompatibility. Powder metallurgy (PM) techniques can be used to fabricate biomaterials with tailored properties because changing the processing parameters, such as the sintering temperature, products with different level of porosity and mechanical performances can be obtained. This study addresses the production of the biomedical Ti-6Al-7Nb alloy by means of the master alloy addition variant of the PM blending elemental approach. The sintering parameters investigated guarantee that the complete diffusion of the alloying elements and the homogenization of the microstructure is achieved. The sintering of the Ti-6Al-7Nb alloy induces a total shrinkage between 7.4% and 10.7% and the level of porosity decreases from 6.2% to 4.7% with the increment of the sintering temperature. Vickers hardness (280–300 HV30) and tensile properties (different combination of strength and elongation around 900 MPa and 3%) are achieved.Item type:Publication, Microstructure and mechanical properties of TiAl alloys produced by rapid heating and open die forging of blended elemental powder compacts2013, ElsevierTi-43Al-5V-4Nb (at%) intermetallic compounds were fabricated by a rapid heating and open die forging method using blended elemental powders. The process route consisted of powder blending, compacting, rapid heating, open die forging and heat treatment. During heating there is porosity in the blended and warm compacted powder billets which still persists after the first forging. In order to remove this difficulty a two stage forging process was used. A fully lamellar structure was seen in the TiAl alloy after heat treatment. Overall, the TiAl alloy showed moderately good mechanical properties at room temperature and good mechanical properties, with reasonable strength and good ductility at high temperatures.Item type:Publication, Modification of sintered titanium alloys by hot isostatic pressing2012, Trans Tech PublicationsPowder metallurgy (PM) permits to obtain titanium alloys with properties and microstructures close to ingot metallurgy products. However, residual porosity is normally present in the products produced by the PM route of powder pressing and sintering (P&S)\, and this needs to be reduced by using post-sintering process step such as hot isostatic pressing (HIP) and forging. In this study, the microstructural and mechanical property changes caused by HIP of samples of two alloys, near-α Ti-3Al-2.5V alloy and α+β Ti-6Al-4V, produced by P&S route were investigated. Two types of powders were utilised: prealloyed powders and blend of elemental titanium powder and master alloy powder. Four conditions defined by HIP temperature, pressure and time were used to HIP the sintered samples with two geometries. The results show that, independent of the HIP conditions used, HIP increased the relative density of the samples to approximately 97.5% and their hardness by 30-50 HV depending on the HIP condition. However, HIP at 1000°C changes the fracture mode of the sintered samples from ductile to brittle.Item type:Publication, Comparison of blended elemental (BE) and mechanical alloyed (MA) powder compact forging into Ti-6Al-4V rocker arms2012, Trans Tech PublicationsTi-6Al-4V rocker arms for internal combustion engines were produced by forging of compacts of blended powder consisting of elemental hydride-dehydride (HDH) titanium powder and Al60V40 (wt%) master alloy powder or mechanical alloyed (MA) powder synthesized by high energy mechanical milling of a mixture of HDH titanium and Al60V40 master alloy powders. The powder compacts were made by warm compaction, and their relative density was 90%. The mechanical properties and microstructures of as-forged parts made using blended powder were improved significantly with increasing holding time at forging temperature, and close to those of as-forged parts produced by powder compact forging of HDH Ti-6Al-4V pre-alloyed powder. However, the as-forged part produced by powder compact forging of MA powder was brittle, and fractured prematurely during tensile testing.Item type:Publication, Tensile properties of Ti-6Al-4V discs produced by open die powder compact forging of pre-alloyed HDH powders2012, Trans Tech PublicationsOpen die powder compact forging was employed for consolidation of Ti-6Al-4V(wt.%) powders which were produced by a hydride-dehydride (HDH) process. The powders were initially warm-compacted into cylindrical shapes. Induction heating was used for preheating the compacts prior to forging into plates. The effect of the forging parameters such as temperature and pre-sintering time on the microstructure and tensile properties of the forged plates were studied. Porosity and the alpha-beta phase distribution were investigated to enable a better understanding of their effect on the fracture behaviour of the tensile tested specimens. The fracture surfaces of the broken tensile specimens were analysed using Scanning Electron Microscopy (SEM) to find the correlation between microstructure, residual porosity and fracture behaviour. A combination of high ultimate tensile strength of over 1200MPa and a good ductility reflected by an elongation to fracture of around 10% was achieved in some of the forged discs.Item type:Publication, Effects of lubrication on the powder metallurgy processing of titanium2012, Trans Tech PublicationsThe role of lubrication on the consolidation behaviour of titanium powder, density increase and change in microstructure on subsequent sintering was investigated. HDH titanium powder mixed with 0-2wt% stearic acid or magnesium stearate was cold compacted. It was found that 0.3-0.6wt% of internal lubricant significantly improves the compressibility. However, more than 0.6wt% of lubricant aids the densification in the low-pressure region but limits the maximum density at high pressure. Moreover, 0.3-0.6wt% of lubricant offers a more uniform density distribution to the powder compact, while greater than 0.6wt% of lubricant leads to a segregation of lubricant in the surface region. The shape retention, ejection behaviour, de-lubrication behaviour and sintered properties were also studied in this work.