<link rel="stylesheet" href="styles.cf390c6bfbe7555f.css">

University of Waikato Research

Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288

Browse

Search Results

Now showing 1 - 5 of 5
  • Item type:Publication,
    On microstructural evolution and mechanical properties of Ti-5Al-5V-5Mo-3Cr alloy synthesised from elemental powder mixtures
    2018, Elsevier
    In this paper, we explored to prepare a multi-compositional titanium alloy, Ti-5Al-5V-5Mo-3Cr (Ti-5553), by powder compact extrusion from elemental powder mixtures, and investigate the microstructure variation during the synthesising process and after post heat treatments and the changes of mechanical properties. XRD, OM and SEM were used to analyse the phase constitutions and microstructures of the Ti-5553 alloy at different processing conditions, and tensile tests were conducted to examine their mechanical properties. The results showed that a homogeneous Ti-5553 alloy was successfully produced by powder compact extrusion from the powder mixtures, β phase was mainly contained in the hot-pressed and 1200°C-extruded Ti-5553 alloy and had an equiaxed microstructure. Different types of α phase precipitated from the β matrix after heat treatment, and this significantly changed the microstructures and improved the mechanical properties of the extruded Ti-5553 alloy, with yield strength of 1250 MPa and ultimate strength of 1300 MPa for the alloy treated at 675 °C for 2 h, and the ductility of about 6.1% for the alloy treated at 780 °C for 2 h.
  • Item type:Publication,
    Evaluation of the mechanical properties of powder metallurgy Ti-6Al-7Nb alloy
    2017-03
    Titanium and its alloys are common biomedical materials owing to their combination of mechanical properties, corrosion resistance and biocompatibility. Powder metallurgy (PM) techniques can be used to fabricate biomaterials with tailored properties because changing the processing parameters, such as the sintering temperature, products with different level of porosity and mechanical performances can be obtained. This study addresses the production of the biomedical Ti-6Al-7Nb alloy by means of the master alloy addition variant of the PM blending elemental approach. The sintering parameters investigated guarantee that the complete diffusion of the alloying elements and the homogenization of the microstructure is achieved. The sintering of the Ti-6Al-7Nb alloy induces a total shrinkage between 7.4% and 10.7% and the level of porosity decreases from 6.2% to 4.7% with the increment of the sintering temperature. Vickers hardness (280–300 HV30) and tensile properties (different combination of strength and elongation around 900 MPa and 3%) are achieved.
  • Item type:Publication,
    Comparison of blended elemental (BE) and mechanical alloyed (MA) powder compact forging into Ti-6Al-4V rocker arms
    2012, Trans Tech Publications
    Ti-6Al-4V rocker arms for internal combustion engines were produced by forging of compacts of blended powder consisting of elemental hydride-dehydride (HDH) titanium powder and Al60V40 (wt%) master alloy powder or mechanical alloyed (MA) powder synthesized by high energy mechanical milling of a mixture of HDH titanium and Al60V40 master alloy powders. The powder compacts were made by warm compaction, and their relative density was 90%. The mechanical properties and microstructures of as-forged parts made using blended powder were improved significantly with increasing holding time at forging temperature, and close to those of as-forged parts produced by powder compact forging of HDH Ti-6Al-4V pre-alloyed powder. However, the as-forged part produced by powder compact forging of MA powder was brittle, and fractured prematurely during tensile testing.
  • Item type:Publication,
    Preparation, microstructure and properties of Ti-6Al-4V rods by powder compact extrusion of powder mixture
    2012, Trans Tech Publications
    Ti-6Al-4V (wt%) alloy rods were prepared successfully using a low-cost method that combines mixing elemental and master alloy powders and powder compact extrusion. The microstructure and mechanical properties of the rods and the effects of extrusion temperature on them were investigated. The results showed that the microstructure and mechanical properties of the extruded rods were strongly affected by the extrusion temperature. With increasing extrusion temperature from 1200°C to 1300°C and keeping the powder compact holding time unchanged at 2 minutes, the fraction of undissolved V rich particles in the microstructure of the extruded rod decreased substantially to zero, the level of composition homogenization increased dramatically to the highest level, and the UTS and elongation of the extruded rods increased significantly from 886MPa and 1.2% to 1300MPa and 7.1%, respectively. The tensile properties of the Ti-6Al-4V alloy rods produced by powder compact extrusion of the powder mixture are comparable to those of Ti-6Al-4V alloy produced by ingot metallurgy and thermomechanical processing.
  • Item type:Publication,
    Mechanical behaviour of Titanium, Ti-6Al-4V (wt %) alloy and Ti-47Al-2Cr (at %) alloy produced using powder compact forging
    2011, Trans Tech Publications
    Powder compact forging was used to produce bulk consolidated titanium and Ti-6Al-4V (wt %) and Ti-47Al-2Cr (at%) alloy disks from hydrogenated and dehydrogenated (HDH) and gas atomised powders (GA) powders (in the case of titanium and Ti-6Al-4V) and a mechanically milled powder (in the case of Ti-47Al-2Cr alloy). The bulk titanium and Ti-6Al-4V (wt %) alloy have been produced by forging of the powder compacts. The Ti-47Al-2Cr (at %) alloy was produced using canned powder compact forging of a Ti/Al/Cr composite powder. The purpose of the present study is to investigate the deformation and fracture behaviour of the bulk consolidated as-forged materials, by conducting tensile testing at room temperature (RT) and examination of the fractured specimens which had near-α, α + β and γ phase structures, respectively. It was found that as-forged bulk titanium disk produced using HDH powder showed a yield point with a yield strength of ~700 MPa and with a considerable amount of ductility. While the as-forged Ti-6Al-4V (wt %) alloy produced using HDH powder, fractured prematurely without any yielding. On the other hand yielding was observed in the as-forged Ti-6Al-4V (wt %) alloy produced using GA powder, showing a yield strength of ~970 MPa and a considerable amount of plastic strain to fracture. The bulk consolidated Ti-47Al-2Cr (at %) alloy also fractured prematurely with fracture strength of ~125 MPa. The mechanical behaviour of the as-forged bulk materials was found to be dependent on several factors such as initial powders used, green density of the powder compact, forging parameters used during forging. It was expected that the entrapped gas in green compacts, absorbed oxygen, porosity and inter-particle bonding play an important role on the quality of the as-forged material, which in turn affected the mechanical behaviour of the bulk material.