    Impact Modification and Fracture Mechanisms of Core-Shell Particle Reinforced Thermoplastic Protein
    2016-08-01, WILEY-V C H VERLAG GMBH
    Mechanical properties and fracture mechanisms of Novatein thermoplastic protein and blends with core–shell particles (CSPs) have been examined. Novatein is brittle with low impact strength and energy-to-break. Epoxy-modifi ed CSPs increase notched and unnotched impact strength, tensile strain-at-break, and energy-to-break, while tensile strength and modulus decrease as CSP content increases. Tg increases slightly with increasing CSP content attributed to physical crosslinking. Changes to mechanical properties are related to the critical matrix ligament thickness and rate of loading. Novatein control samples display brittle fracture characterized by large-scale crazing. At high CSP content a large plastic zone and a slow crack propagation zone in unnotched and tensile samples are observed suggesting increased energy absorption. Notched impact samples reach critical craze stresses easily regardless of CSP content reducing impact strength. It is concluded that the impact strength of thermoplastic protein can be modifi ed in a similar manner to traditional thermoplastics.
  • Item type:Publication,
    Potential of cellulose microfibers for PHA and PLA biopolymers reinforcement.
    2020, MDPI
    Cellulose nanocrystals (CNC) have attracted the attention of many engineering fields and offered excellent mechanical and physical properties as polymer reinforcement. However, their application in composite products with high material demand is complex due to the current production costs. This work explores the use of cellulose microfibers (MF) obtained by a straightforward water dispersion of kraft paper to reinforce polyhydroxyalkanoate (PHA) and polylactic acid (PLA) films. To assess the influence of this type of filler material on the properties of biopolymers, films were cast and reinforced at different scales, with both CNC and MF separately, to compare their effectiveness. Regarding mechanical properties, CNC has a better reinforcing effect on the tensile strength of PLA samples, though up to 20 wt.% of MF may also lead to stronger PLA films. Moreover, PHA films reinforced with MF are 23% stronger than neat PHA samples. This gain in strength is accompanied by an increment of the stiffness of the material. Additionally, the addition of MF leads to an increase in the crystallinity of PHA that can be controlled by heat treatment followed by quenching. This change in the crystallinity of PHA affects the hygroscopicity of PHA samples, allowing the modification of the water barrier properties according to the required features. The addition of MF to both types of polymers also increases the surface roughness of the films, which may contribute to obtaining better interlaminar bonding in multi-layer composite applications. Due to the partial lignin content in MF from kraft paper, samples reinforced with MF present a UV blocking effect. Therefore, MF from kraft paper may be explored as a way to introduce high fiber concentrations (up to 20 wt.%) from other sources of recycled paper into biocomposite manufacturing with economic and technical benefits.
  • Item type:Publication,
    Short-Term viscoelastic properties of bloodmeal-based thermoplastics
    2014, Wiley
    The effects of sodium sulfite (SS) content and injection molding temperature on the viscoelasticity of bloodmeal-based thermoplastics were assessed using creep, recovery, and stress relaxation. Both SS and processing temperature affected standard mechanical properties and time-dependent behavior. Increased SS content led to greater creep, greater strain at break, and reduced modulus and mechanical strength of the material. Furthermore, the use of a higher injection molding temperature also reduced modulus and strength. Higher molding temperature also caused an increase in the fraction of creep recovered in 20 min. These results confirmed that increased SS increased chain mobility and that injection molding at 140°C instead of 120°C did not cause excessive thermal cross-linking.
  • Item type:Publication,
    Injection-Molding Performance and Mechanical Properties of Blood Meal-Based Thermoplastics
    2013, Wiley
    Protein-based thermoplastics offer an attractive alternative to petroleum-based plastics if their properties allow for large volume production using processes such as injection molding. A fractional factorial design was used to analyze the influence of injection-molding parameters (melt temperature, tool temperature, injection rate, holding pressure, and cooling time) on the injection-molding process (maximum injection pressure, injection pressure curve) and mechanical properties (tensile strength, elongation at break, secant modulus) of blood meal–based thermoplastics. Optimal mechanical properties were obtained at higher tool and melt temperatures while the injection rate was unimportant. The most important injection parameter was the holding pressure, which has to be lowered when using a higher melt temperature, which was preferred for better elongation at break. A lower holding pressure also produced moldings with a higher modulus, which could be good for demolding. Blood meal–based thermoplastics behaved mostly like standard thermoplastics, without any significant deviations. Within a workable processing window, its mechanical properties were largely unaffected by processing conditions, but as with any thermoplastic, care must be taken to select the best injection-molding parameter settings to achieve optimal part quality and high processability.
  • Item type:Publication,
    Structural changes as a result of processing in thermoplastic bloodmeal
    2012, Wiley
    Bloodmeal (BM) can be thermoplastically processed resulting in a material with good mechanical properties by using a correct combination of additives. In this article, combinations of water, sodium sulfite (SS), sodium dodecyl sulfate (SDS), and urea were compounded with BM, and water absorption, solubility, thermal stability, and protein secondary structure were assessed. Thermal stability of processed plastics was reduced when using 2 or 3 pphbm (parts per hundred parts BM) SS and 20 pphbm urea, mostly indicative of a reduction in covalent crosslinking. SS was required for chain mobility during processing, however, without sufficient plasticization degradation will occur instead of melt formation. SDS further improved processability and consolidation leading to increased water absorption and solubility, indicative of a reduction in chain interactions. It was found that BM proteins are highly denatured and thermoplastic processing reduced ordered structures further. Additional minor structural changes occurred as a result of reduced covalent and noncovalent interactions after processing. It was concluded that the increase in water absorption and solubility was due to changes in intermolecular and intramolecular interactions, rather than substantial structural changes.