  • Item type:Publication,
    The manufacture and mechanical properties of aligned long harakeke fibre reinforced epoxy composites
    2012-07-09
    Aligned long harakeke fibre reinforced epoxy composites were prepared using hand lay-up followed by compression moulding. Densities of harakeke fibre and epoxy resin were determined for the purpose of composite design. The evenness of composites fabricated by two different size moulds was compared. It was found that more even composites were produced when using a small mould than a big mould. In this work, the dependence of tensile and flexural properties of harakeke/epoxy composites on fibre content was also investigated. The results showed that the addition of fibre enhanced tensile properties of epoxy. The tensile strength and Young’s modulus increased with the volume fraction of harakeke fibre. The flexural strength and flexural modulus increased as the fibre volume fraction increased up to 0.4. Further addition of fibre did not result in an improvement of composite flexural properties.
  • Item type:Publication,
    Influence of alkali fiber treatment and fiber processing on the mechanical properties of hemp/epoxy composites
    2010-10, Wiley
    Industrial hemp fibers were treated with a 5 wt % NaOH, 2 wt % Na₂SO₃ solution at 120°C for 60 min to remove noncellulosic fiber components. Analysis of fibers by lignin analysis, scanning electron microscopy (SEM), zeta potential, Fourier transform infrared (FTIR) spectroscopy, wide angle X-ray diffraction (WAXRD) and differential thermal/thermogravimetric analysis (DTA/TGA), supported that alkali treatment had (i) removed lignin, (ii) separated fibers from their fiber bundles, (iii) exposed cellulose hydroxyl groups, (iv) made the fiber surface cleaner, and (v) enhanced thermal stability of the fibers by increasing cellulose crystallinity through better packing of cellulose chains. Untreated and alkali treated short (random and aligned) and long (aligned) hemp fiber/epoxy composites were produced with fiber contents between 40 and 65 wt %. Although alkali treatment generally improved composite strength, better strength at high fiber contents for long fiber composites was achieved with untreated fiber, which appeared to be due to less fiber/fiber contact between alkali treated fibers. Composites with 65 wt % untreated, long aligned fiber were the strongest with a tensile strength (TS) of 165 MPa, Young's modulus (YM) of 17 GPa, flexural strength of 180 MPa, flexural modulus of 9 GPa, impact energy (IE) of 14.5 kJ/m², and fracture toughness (KIc) of 5 MPa m1/2