    Effect of fibre treatments on interfacial shear strength of hemp fibre reinforced polylactide and unsaturated polyester composites
    2011, Elsevier
    Surface treatment of hemp fibres was investigated as a means of improving interfacial shear strength (IFSS) of hemp fibre reinforced polylactide (PLA) and unsaturated polyester (UPE) composites. Fibres were treated with sodium hydroxide, acetic anhydride, maleic anhydride and silane. A combined treatment using sodium hydroxide and silane was also carried out. IFSS of PLA/hemp fibre samples increased after treatment, except in the case of maleic anhydride treatment. Increased IFSS could be explained by better bonding of PLA with treated fibres and increased PLA transcrystallinity. The highest IFSS was 11.4 MPa which was obtained for the PLA/alkali treated fibre samples. IFSS of UPE/hemp fibre samples increased for all treated fibres. This is believed to be due to the improvement of chemical bonding between the treated fibres and the UPE as supported by FT-IR results. The highest IFSS (20.3 MPa) was found for the combined sodium hydroxide and silane treatment fibre/UPE samples.
  • Item type:Publication,
    Hemp fibre reinforced composites using chelator and enzyme treatments
    2010, Elsevier
    The main objective of the current work was to investigate using chelator treatment, and combined chelator and enzyme treatments, to separate hemp fibre from its bundles, as well as remove non-cellulosic compounds, and thus therefore improve the interfacial bonding in the composite. Wet chemical analysis, FTIR, X-ray diffraction (XRD), thermal analysis and single fibre tensile testing were used to characterise the effect of treatment on hemp fibres. The higher chelator concentration treated hemp fibre composites had the highest tensile strength of 42 MPa, an increase of 19% compared to composites with untreated hemp fibre.
  • Item type:Publication,
    Modification of kraft wood-pulp fibre with silica for surface functionalisation
    2008, Elsevier
    A new science strategy for natural fibre modification was devised in which glass surface properties would be imparted to wood-derived fibre. The enhancements known from addition of silane reagents to glass fibre–polymer composites could therefore be realised for modified cellulose fibre–polymer composites. A process is described whereby the internal void spaces and micropores of never-dried Kraft pulp fibre walls were impregnated with silica. This was achieved by initial dehydration of never-dried fibre through azeotropic distillation to achieve substitution of fibre water with the silicon chemical solution over a range of concentrations. Kraft fibres were stiffened and made resistant to collapse from the effect of the azeotrope drying. Specific chemical reaction of azeotrope-dried fibre with the reagent ClSi(OEt)3 followed by base-catalysed hydrolysis of the ester groups formed a fibre-bound silica composite. The physico-chemical substitution of water from micropores and internal voids of never-dried fibre with property-modifying chemicals offers possibilities in the development of new fibre characteristics, including fibres which may be hardened, plasticised, and/or stabilised against moisture, biodegradation or fire. The embedded silica may also be used as sites of attachment for coupling agents to modify the hydrophilic character of the fibre or to functionalise the fibre surface.