University of Waikato Research
Permanent URI for this communityhttps://researchcommons.waikato.ac.nz/handle/10289/10288
Browse
4 results
Search Results
Item type:Publication, Influence of loading rate, alkali fibre treatment and crystallinity on fracture toughness of random short hemp fibre reinforced polylactide bio-composites2011, ElsevierPlane-strain fracture toughness (KIc) of random short hemp fibre reinforced polylactide (PLA) bio-composites was investigated along with the effect of loading rate, fibre treatment and PLA crystallinity. Fracture toughness testing was carried out at loading rates varying from 0.5 to 20 mm/min using single-edge-notched bending specimens with 0 to 30 wt% fibre. KQ (trial KIc) of composites decreased as loading rate increased, until stabilising to give KIc values at a loading rate of 10 mm/min and higher. The reduction of crazing and stress whitening, as well as a more direct crack path observed in PLA samples combined with reduced plastic deformation observed in composites provided explanation for this reduction. KIc of composites was found to decrease with increased fibre content and fibre treatment with sodium hydroxide. Studies controlling the degree of PLA crystallinity by heat treatment or “annealing” showed that reduction of KIc can be attributed to increased crystallinity.Item type:Publication, Influence of hygrothermal ageing on the physico-mechanical properties of alkali treated industrial hemp fibre reinforced polylactic acid composites2010, SpringerLink30 wt% aligned untreated long hemp fibre/polylactic acid (AUL) and aligned alkali treated long hemp fibre/polylactic acid (AAL) composites were produced by film stacking and subjected to hygrothermal ageing environment along with neat polylactic acid (PLA). Hygrothermal ageing was carried out by immersing samples in distilled water at 25 and 50 ºC over a period of 3 months. It was found that both neat PLA and composites followed Fickian diffusion. Higher temperature generally increased the Diffusion coefficient, D of neat PLA and composites, as well as shortening the saturation time. Neat PLA had the lowest D value followed by AAL composites and then AUL composites. After hygrothermal ageing, tensile and flexural strength, Young’s and flexural modulus and KIc were found to decrease and impact strength was found to increase for both AUL and AAL composites. AUL composites had greater overall reduction in mechanical properties than that for AAL composites after hygrothermal ageing. Crystallinity contents of the hygrothermal aged composites support the results of the deterioration of mechanical properties upon exposure to hygrothermal ageing environment.Item type:Publication, Characterisation of hemp fibre reinforced Poly(Lactic Acid) composites2009, Inderscience EnterprisesIn this work, the mechanical properties including tensile strength, flexural strength, impact strength and fracture toughness of the PLA/hemp composites were investigated over a range of fibre content (0-30 wt.%). It was observed that, the tensile strength and Young's modulus of the composites increased with increased fibre content. The flexural strength did not increase with fibre reinforcement, however, the flexural modulus of the composites increased significantly. Impact strength of the composites increased up to 20 wt. % fibre loading, however, further increased fibre loading caused a reduction of impact strength. KIc and GIc values decreased with increased fibre content.Item type:Publication, Influence of accelerated ageing on the physico-mechanical properties of alkali-treated industrial hemp fibre reinforced poly(lactic acid) (PLA) composites2010, Elsevier30 wt% aligned untreated long hemp fibre/PLA (AUL) and aligned alkali treated long hemp fibre/PLA (AAL) composites were produced by film stacking and subjected to accelerated ageing. Accelerated ageing was carried out using UV irradiation and water spray at 50 °C for four different time intervals (250, 500, 750 and 1000 h). After accelerated ageing, tensile strength (TS), flexural strength, Young's modulus (YM), flexural modulus and mode I fracture toughness (KIc) were found to decrease and impact strength (IS) was found to increase for both AUL and AAL composites. AUL composites had greatest overall reduction in mechanical properties than that for AAL composites upon exposure to accelerated ageing environment. FTIR analysis and crystallinity contents of the accelerated aged composites support the results of the deterioration of mechanical properties upon exposure to accelerated ageing environment.