  • Item type:Publication,
    Fabrication, microstructure, mechanical, and electrochemical properties of NiMnFeCu high entropy alloy from elemental powders
    2022, MDPI AG
    Transition metal based high entropy alloys (HEAs) are often used in electrocatalytic (water electrolysis) applications due to the synergistic effect operating among its constituent elements and unpaired electrons in d orbitals of the concerned metal. In this study, a low cost NiMnFeCu high entropy alloy was successfully synthesised using the combined techniques of mechanical milling (MA) and vacuum sintering. X‐ray diffraction was used to analyse the phase composition, optical microscopy, and scanning electron microscopy were used to characterise the fabricated material’s microstructure and chemical homogeneity, thermal, and mechanical properties were tested using the differential scanning calorimetry method and a universal testing machine, respectively. Electrochemical workstation was used to carry out preliminary electrochemical studies such as linear sweep voltammetry (LSV), cyclic voltammetry (CV) and chronoamperometry. The results showed that the as‐ sintered NiMnFeCu HEA possessed a single‐ phase FCC structure. The HEA NiMnFeCu sintered at 1050 °C (S4) and 1000 °C (S2) with a holding time of 2 h showed a yield strength of 516.3 MPa and 389.8 MPa, respectively, and the micro‐hardness values were measured to be 233.45 ± 9 HV and 198.7 ± 8 HV, respectively. Preliminary electrochemical studies proved that the alloy sintered at 1000 °C (S2) with a holding time of 2 h exhibited excellent electrocatalytic properties with a measured overpotential of 322 mV at 10 mA cm⁻² at 100 cycles of CV and good stability for 10 h when compared to state‐of‐the‐art electrocatalytic materials IrO₂ and RuO₂ This suggested that the HEA NiMnFeCu fabricated under the condition S2 could potentially be used for industrial‐scale water electrolysis as it possesses permissible mechanical and good electrochemical properties.
  • Item type:Publication,
    Heat treatment, impact properties, and fracture behaviour of Ti-6Al-4V alloy produced by powder compact extrusion.
    2019, MDPI
    The mechanical properties of titanium and titanium alloys are very sensitive to processing, microstructure, and impurity levels. In this paper, a blended powder mixture of Ti-6Al-4V alloy was consolidated by powder compact extrusion that involved warm compaction, vacuum sintering, and hot extrusion. The as-processed material with an oxygen content of 0.34 wt.% was subjected to various annealing treatments. The impact toughness of heat-treated material was determined using Charpy V-notch impact testing at room temperature. An emphasis was placed on establishing a relationship among fracture behaviour, microstructure, and the resulting properties of tested material. From the results, it is apparent that the highest impact toughness value of 19.3 J was achieved after α/β annealing and is comparable with typical values given in the literature for wrought Ti-6Al-4V. In terms of fracture behaviour, it is quite apparent that the crack propagation behaviour of powder-produced material is rather complex compared with the limited amount of data reported for ingot counterparts.
  • Item type:Publication,
    Effect of microwave sintering parameters on the physical and mechanical properties of pure Ti and blended elemental Ti alloys
    2018, Trans Tech Publications
    Microwave sintering (MWS) was used to consolidate hydride de-hydride Ti powder and blended elemental Ti6Al4V, Ti5Fe and Ti5Al5Mo5V3Cr (Ti5553) powder mixtures. The amount of powders used to prepare the powder compacts was scaled up to 500g.The effect of the MWS conditions on the relative density, porosity distribution, microstructure and tensile properties were studied. Furthermore, uniformity in distribution of the alloying elements was checked. For most of the materials considered, a combinations of sintering temperature of 1200ºC and 1300ºC and holding time of 5 to 30 min resulted in significantly improved density. Nevertheless sintering temperature of at least 1300ºC was required for pore coalescence and high tensile properties.
  • Item type:Publication,
    Sensitive pyroclastic soils in the Bay of Plenty, New Zealand: microstructure to failure mechanisms
    2017, New Zealand Geotechnical Society
    Sensitive soils derived from weathered rhyolitic pyroclastic materials are associated with many landslides in the Bay of Plenty. Undrained, consolidated static triaxial tests show contractive p’-q’ plots, strain-softening stress-strain behaviour coupled with rising pore water pressures, shear band formation after peak strength, and considerable strain softening. Cyclic triaxial tests confirm brittle failure and extensive softening of the soil. Pore pressure gradients developed during shearing initiate collapse of clay microstructures into shear zones; further excess pore pressure generation in the shear zone leads to progressive failure. Halloysite, a low-activity clay mineral, is associated with sensitive layers within the pyroclastic sequences. Mushroom cap–shaped spheroidal halloysite results in weak short-range interactions between exposed clay surfaces on incomplete spheroids. This weak bonding allows disassociation of clay aggregates during slope failure, leading to strain softening and the development of flow post-failure.
  • Item type:Publication,
    Sintering behaviour and microstructures of Ti(Al,O)/Al₂O₃, Ti₃Al(O)/Al₂O₃ and TiAl(O)/Al₂O₃ in situ composites
    2006, Elsevier
    The sintering behaviour and microstructures of Ti(Al,O)/Al₂O₃, Ti₃Al(O)/Al₂O₃ and TiAl(O)/Al₂O₃ in situ composites produced using Al/TiO₂ composite powders have been studied. Ti(Al,O), Ti₃Al(O) and TiAl(O) represent α-Ti phase with dissolved Al and O, and Ti3Al and TiAl phases with dissolved O, respectively. The Al/TiO₂ composite powders were produced by high energy mechanical milling using Al and TiO₂ powders as the starting materials. It was found that the matrices of the composites became fully dense after sintering at 1550 °C, and the Al₂O₃ particles became fully sintered when the sintering temperature was increased to 1650 °C. The reactions between Al and TiO₂ which occur during heating the powder compacts to 1400 °C have little effect on the sintering of the composite powders. The Al₂O₃ particles in the composites become significantly coarsened during sintering at 1550 °C or above, and the coarsening rate of the Al₂O₃ particles increases in the order of Ti(Al,O)/Al₂O₃, Ti₃Al(O)/Al₂O₃ and TiAl/Al₂O₃ composites. This can be attributed to the decrease of the solidus temperature or melting points of the corresponding matrices. It is evident that in the initial stage of sintering, coarsening of the Al2O₃ particles occurs through coalescence. Hipping of the pre-sintered composites at 1300 °C with a pressure of 200 MPa without canning causes significant increase of the density and substantial further coarsening of the Al₂O₃ particles.
  • Item type:Publication,
    Microstructure and mechanical properties of TiAl alloys produced by rapid heating and open die forging of blended elemental powder compacts
    2013, Elsevier
    Ti-43Al-5V-4Nb (at%) intermetallic compounds were fabricated by a rapid heating and open die forging method using blended elemental powders. The process route consisted of powder blending, compacting, rapid heating, open die forging and heat treatment. During heating there is porosity in the blended and warm compacted powder billets which still persists after the first forging. In order to remove this difficulty a two stage forging process was used. A fully lamellar structure was seen in the TiAl alloy after heat treatment. Overall, the TiAl alloy showed moderately good mechanical properties at room temperature and good mechanical properties, with reasonable strength and good ductility at high temperatures.
  • Item type:Publication,
    Microstructure and mechanical properties of large size as-cast Ti-43Al-9V-0.2Y (at.%) alloy ingot from brim to centre
    2011, Elsevier
    A Ti-43Al-9V-0.2Y (at.%) alloy ingot with the size of Ф160×400mm was prepared by vacuum arc remelting (VAR). The microstructure of the as-cast Ti-43Al-9V-0.2Y alloy was composed of B2/α₂/γ lamellar colonies and massive B2 and γ phases which were distributed along the boundaries of these lamellar colonies in the form of equiaxed grains. Based on the grain size variation along the radius direction of the ingot, the ingot could be divided into four ring regions from brim to centre. It has been understood that the grain size variation between these four regions was due to the interplay of the effects of the cooling rate and the yttrium content on solidified microstructures in these regions. Mechanical testing of the samples cut from these four regions showed that there existed a clear correlation between the yield strength and the average grain sizes of the four ring regions, which approximately conformed to a Hall-Petch relationship.
  • Item type:Publication,
    Interfacial microstructure and shear strength of Ti-6Al-4V/TiAl laminate composite sheet fabricated by hot packed rolling
    2011, Elsevier
    A two layer Ti-6Al-4V(wt%)/Ti-43Al-9V-Y(at%) laminate composite sheet with a uniform interfacial microstructure and no discernible defects at the interfaces has been prepared by hot-pack rolling, and its interfacial microstructure and shear strength were characterized. Characterization of the interfacial microstructure shows that there was an interfacial region of uniform thickness of about 250 μm which consisted of two layers: Layer I on the TiAl side which was 80 μm thick and Layer II on the Ti-6Al-4V side which was 170 μm thick. The microstructure of Layer I consisted of massive γ phases, needlelike γ phases and B2 phase matrix, while the microstructure of Layer II consisted of α₂ phase. The microstructure of the interfacial region is the result of the interdiffusion of Ti element from Ti-6Al-4V alloy layer into the TiAl alloy layer and Al element from the TiAl alloy layer into the Ti-6Al-4V alloy layer. The shear strength measurement demonstrated that the bonding strength between the TiAl alloy and Ti-6Al-4V alloy layers in the laminate composite sheet was very high. This means that the quality of the interfacial bonding between the two layers achieved by the multi-path rolling is high, and the interface between the layers is very effective in transferring loading, causing significantly improved toughness and plasticity of the TiAl/Ti-6Al-4V laminate composite sheet.