    Sintering behaviour and microstructures of Ti(Al,O)/Al₂O₃, Ti₃Al(O)/Al₂O₃ and TiAl(O)/Al₂O₃ in situ composites
    2006, Elsevier
    The sintering behaviour and microstructures of Ti(Al,O)/Al₂O₃, Ti₃Al(O)/Al₂O₃ and TiAl(O)/Al₂O₃ in situ composites produced using Al/TiO₂ composite powders have been studied. Ti(Al,O), Ti₃Al(O) and TiAl(O) represent α-Ti phase with dissolved Al and O, and Ti3Al and TiAl phases with dissolved O, respectively. The Al/TiO₂ composite powders were produced by high energy mechanical milling using Al and TiO₂ powders as the starting materials. It was found that the matrices of the composites became fully dense after sintering at 1550 °C, and the Al₂O₃ particles became fully sintered when the sintering temperature was increased to 1650 °C. The reactions between Al and TiO₂ which occur during heating the powder compacts to 1400 °C have little effect on the sintering of the composite powders. The Al₂O₃ particles in the composites become significantly coarsened during sintering at 1550 °C or above, and the coarsening rate of the Al₂O₃ particles increases in the order of Ti(Al,O)/Al₂O₃, Ti₃Al(O)/Al₂O₃ and TiAl/Al₂O₃ composites. This can be attributed to the decrease of the solidus temperature or melting points of the corresponding matrices. It is evident that in the initial stage of sintering, coarsening of the Al2O₃ particles occurs through coalescence. Hipping of the pre-sintered composites at 1300 °C with a pressure of 200 MPa without canning causes significant increase of the density and substantial further coarsening of the Al₂O₃ particles.
  • Item type:Publication,
    Transient liquid phase sintering of high density Transient liquid phase sintering of high density Fe₃Al using Fe and Fe₂Al₅/FeAl₂ powders Part 1: Experimentation and results
    2003-03, Maney Publishing
    High density Fe[sub 3]Al was produced through transient liquid phase sintering, using rapid heating rates of greater than 150 K min[sup -1] and a mixture of prealloyed and elemental powders. Prealloyed Fe[sub 2]Al[sub 5]/FeAl[sub 2] (50Fe/50Al, wt-%) powder was added to elemental iron powder in a ratio appropriate for producing an overall Fe[sub 3]Al (13•87 wt-%) ratio. The heating rate, sintering time, sintering temperature, green density and powder particle size were controlled during the study. Heating rate, sintering time and powder particle size had the most significant influence upon the sintered density of the compacts. The highest sintered density of 6•12 Mg m[sup -3] (92% of the theoretical density for Fe3Al) was achieved after 15 minutes of sintering at 1350°C, using a 250 K min[sup - 1] heating rate, 1-6 μm Fe powders and 5•66 μm alloy powders. SEM microscopy suggests that agglomerated Fe[sub 2]Al[sub 5]/ FeAl[sub 2] particles, which form a liquid during sintering, are responsible for a significant portion of the remaining porosity in high sintered density compacts, creating stable pores, larger than 100 μm diameter, after melting. High density was achieved by minimising the Kirkendall porosity formed during heating by unbalanced diffusion and solubility between the iron and Fe[sub 2]Al[sub 5]/FeAl[sub 2] components. The lower diffusion rate of aluminium in the prealloyed powder into the iron compared with elemental aluminium in iron, coupled with a fast heating rate, is expected to permit minimal iron-aluminium interdiffusion during heating so that when a liquid forms the aluminium dissolves in the iron to promote solidification at a lower aluminium content. This leads to a further reduction in porosity.